1.
In this study the thickness of the PTB7‐Th:PC71BM bulk heterojunction (BHJ) film and the PF3N‐2TNDI electron transport layer (ETL) is systematically tuned to achieve polymer solar cells (PSCs) with optimized power conversion efficiency (PCE) of over 9% when an ultrathin BHJ of 50 nm is used. Optical modeling suggests that the high PCE is attributed to the optical spacer effect from the ETL, which not only maximizes the optical field within the BHJ film but also facilitates the formation of a more homogeneously distributed charge generation profile across the BHJ film. Experimentally it is further proved that the extra photocurrent produced at the PTB7‐Th/PF3N‐2TNDI interface also contributes to the improved performance. Taking advantage of this high performance thin film device structure, one step further is taken to fabricate semitransparent PSCs (ST‐PSCs) by using an ultrathin transparent Ag cathode to replace the thick Ag mirror cathode, yielding a series of high performance ST‐PSCs with PCEs over 6% and average visible transmittance between 20% and 30%. These ST‐PSCs also possess remarkable transparency color perception and rendering properties, which are state‐of‐the‐art and fulfill the performance criteria for potential use as power‐generating windows in near future.  相似文献   

2.
Development of high‐performance donor–acceptor (D–A) copolymers is vital in the research of polymer solar cells (PSCs). In this work, a low‐bandgap D–A copolymer based on dithieno[3,2‐b:2′,3′‐d]pyridin‐5(4H)‐one unit (DTP), PDTP4TFBT, is developed and used as the donor material for PSCs with PC71BM or ITIC as the acceptor. PDTP4TFBT:PC71BM and PDTP4TFBT:ITIC solar cells give power conversion efficiencies (PCEs) up to 8.75% and 7.58%, respectively. 1,8‐Diiodooctane affects film morphology and device performance for fullerene and nonfullerene solar cells. It inhibits the active materials from forming large domains and improves PCE for PDTP4TFBT:PC71BM cells, while it promotes the aggregation and deteriorates performance for PDTP4TFBT:ITIC cells. The ternary‐blend cells based on PDTP4TFBT:PC71BM:ITIC (1:1.2:0.3) give a decent PCE of 9.20%.  相似文献   

3.
Perylene diimide (PDI) with high electron affinities are promising candidates for applications in polymer solar cells (PSCs). In addition, the strength of π‐deficient backbones and end‐groups in an n‐type self‐dopable system strongly affects the formed end‐group‐induced electronic interactions. Herein, a series of amine/ammonium functionalized PDIs with excellent alcohol solubility are synthesized and employed as electron transporting layers (ETLs) in PSCs. The electron transfer properties of the resulting PDIs are dramatically tuned by different end‐groups and π‐deficient backbones. Notably, electron transfer is observed directly in solution in self‐doped PDIs for the first time. A significantly enhanced power conversion efficiency of 10.06% is achieved, when applying the PDIs as ETLs in PTB7‐Th:PC71BM‐based PSCs. These results demonstrate the potential of n‐type organic semiconductors with stable n‐type doping capability and facile solution processibility for future applications of energy transition devices.  相似文献   

4.
A universal strategy for efficient light trapping through the incorporation of gold nanorods on the electron transport layer (rear) of organic photovoltaic devices is demonstrated. Utilizing the photons that are transmitted through the active layer of a bulk heterojunction photovoltaic device and would otherwise be lost, a significant enhancement in power conversion efficiency (PCE) of poly[N‐9′‐heptadecanyl‐2,7‐carbazole‐alt‐5,5‐(4′,7′‐di‐2‐thienyl‐2′,1′,3′‐benzothiadiazole)]:phenyl‐C71‐butyric acid methyl ester (PCDTBT:PC71BM) and poly[[4,8‐bis[(2‐ethylhexyl)oxy]benzo[1,2‐b:4,5‐b′]dithiophene‐2,6‐diyl][3‐fluoro‐2‐[(2‐ethylhexyl)carbonyl]thieno[3,4‐b] thiophenediyl]] (PTB7):PC71BM by ≈13% and ≈8%, respectively. PCEs over 8% are reported for devices based on the PTB7:PC71BM blend. A comprehensive optical and electrical characterization of our devices to clarify the influence of gold nanorods on exciton generation, dissociation, charge recombination, and transport inside the thin film devices is performed. By correlating the experimental data with detailed numerical simulations, the near‐field and far‐field scattering effects are separated of gold nanorods (Au NRs), and confidently attribute part of the performance enhancement to the enhanced absorption caused by backscattering. While, a secondary contribution from the Au NRs that partially protrude inside the active layer and exhibit strong near‐fields due to localized surface plasmon resonance effects is also observed but is minor in magnitude. Furthermore, another important contribution to the enhanced performance is electrical in nature and comes from the increased charge collection probability.  相似文献   

5.
An aromatic lactam acceptor unit, thieno[3,2‐c]isoquinolin‐5(4H)‐one (TIQ), is developed. Compared with its analogues, dithieno[3,2‐b:2′,3′‐d]pyridin‐5(4H)‐one (DTP) and phenanthridin‐6(5H)‐one (PN), TIQ shows its advantage in constructing donor–acceptor (D–A) copolymers for efficient solar cells. TIQ‐based D–A copolymer PTIQ4TFBT delivers a power conversion efficiency (PCE) of 10.16% in polymer:fullerene solar cells, while those based on DTP and PN copolymers, PDTP4TFBT and PPN4TFBT, afford PCEs around 8.5%. The higher performance of PTIQ4TFBT:PC71BM solar cells originates from enhanced short‐circuit current density (Jsc) and fill factor (FF), because of favorable morphology, less bimolecular recombination, and balanced charge transport in the active layer. Moreover, the performance for PTIQ4TFBT:PC71BM solar cells is less sensitive to active layer thickness than PDTP4TFBT:PC71BM and PPN4TFBT:PC71BM solar cells. Over 8% PCEs can be obtained from PTIQ4TFBT:PC71BM solar cells when the active layer thickness is over 500 nm.  相似文献   

6.
Solution‐processed small molecule (SM) solar cells have the prospect to outperform their polymer‐fullerene counterparts. Considering that both SM donors/acceptors absorb in visible spectral range, higher expected photocurrents should in principle translate into higher power conversion efficiencies (PCEs). However, limited bulk‐heterojunction (BHJ) charge carrier mobility (<10‐4 cm2 V‐1 s‐1) and carrier lifetimes (<1 µs) often impose active layer thickness constraints on BHJ devices (≈100 nm), limiting external quantum efficiencies (EQEs) and photocurrent, and making large‐scale processing techniques particularly challenging. In this report, it is shown that ternary BHJs composed of the SM donor DR3TBDTT (DR3), the SM acceptor ICC6 and the fullerene acceptor PC71BM can be used to achieve SM‐based ternary BHJ solar cells with active layer thicknesses >200 nm and PCEs nearing 11%. The examinations show that these remarkable figures are the result of i) significantly improved electron mobility (8.2 × 10‐4 cm2 V‐1 s‐1), ii) longer carrier lifetimes (2.4 µs), and iii) reduced geminate recombination within BHJ active layers to which PC71BM has been added as ternary component. Optically thick (up to ≈500 nm) devices are shown to maintain PCEs >8%, and optimized DR3:ICC6:PC71BM solar cells demonstrate long‐term shelf stability (dark) for >1000 h, in 55% humidity air environment.  相似文献   

7.
Enhanced power conversion efficiency (PCE) is reported in inverted polymer solar cells when an electron‐rich polymer nanolayer (poly(ethyleneimine) (PEI)) is placed on the surface of an electron‐collecting buffer layer (ZnO). The active layer is made with bulk heterojunction films of poly[[4,8‐bis[(2‐ethylhexyl)oxy]benzo[1,2‐b:4,5‐b′]dithiophene‐2,6‐diyl][3‐fluoro‐2‐[(2‐ethylhexyl)carbonyl]thieno[3,4‐b]thiophenediyl]] (PTB7) and [6,6]‐phenyl‐C71‐butyric acid methyl ester (PC71BM). The thickness of the PEI nanolayer is controlled to be 2 nm to minimize its insulating effect, which is confirmed by X‐ray photoelectron spectroscopy and optical absorption measurements. The Kelvin probe and ultraviolet photoelectron spectroscopy measurements demonstrate that the enhanced PCE by introducing the PEI nanolayer is attributed to the lowered conduction band energy of the ZnO layer via the formation of an interfacial dipole layer at the interfaces between the ZnO layer and the PEI nanolayer. The PEI nanolayer also improves the surface roughness of the ZnO layer so that the device series resistance can be noticeably decreased. As a result, all solar cell parameters including short circuit current density, open circuit voltage, fill factor, and shunt resistance are improved, leading to the PCE increase up to ≈8.9%, which is close to the best PCE reported using conjugated polymer electrolyte films.  相似文献   

8.
Polymer solar cells (PSCs) are fabricated without solvent additives using a low‐bandgap polymer, PBDTTT‐C‐T, as the donor and [6,6]‐phenyl‐C61‐butyric‐acid‐methyl‐ester (PC61BM) as the acceptor. Donor‐acceptor blend and layer‐by‐layer (LL) solution process are used to form active layers. Relative to the blend devices, the LL devices exhibit stronger absorption, better vertical phase separation, higher hole and electron mobilities, and better charge extraction at correct electrodes. As a result, after thermal annealing the LL devices exhibit an average power conversion efficiency (PCE) of 6.86%, which is much higher than that of the blend devices (4.31%). The best PCE of the LL devices is 7.13%, which is the highest reported for LL processed PSCs and among the highest reported for PC61BM‐based single‐junction PSCs.  相似文献   

9.
All‐polymer solar cells (all‐PSCs) utilizing p‐type polymers as electron‐donors and n ‐typepolymers as electron‐acceptors have attracted a great deal of attention, and their efficiencies have been improved considerably. Here, five polymer donors with different molecular orientations are synthesized by random copolymerization of 5‐fluoro‐2,1,3‐benzothiadiazole with different relative amounts of 2,2′‐bithiophene (2T) and dithieno[3,2‐b;2′,3′‐d]thiophene (DTT). Solar cells are prepared by blending the polymer donors with a naphthalene diimide‐based polymer acceptor (PNDI) or a [6,6]‐phenyl C71‐butyric acid methyl ester (PC71BM) acceptor and their morphologies and crystallinity as well as optoelectronic, charge‐transport and photovoltaic properties are studied. Interestingly, charge generation in the solar cells is found to show higher dependence on the crystal orientation of the donor polymer for the PNDI‐based all‐PSCs than for the conventional PC71BM‐based PSCs. As the population of face‐on‐oriented crystallites of the donor increased in PNDI‐based PSC, the short‐circuit current density (JSC) and external quantum efficiency of the devices are found to significantly improve. Consequently, device efficiency was enhanced of all‐PSC from 3.11% to 6.01%. The study reveals that producing the same crystal orientation between the polymer donor and acceptor (face‐on/face‐on) is important in all‐PSCs because they provide efficient charge transfer at the donor/acceptor interface.  相似文献   

10.
Molecular orientation, with respect to donor/acceptor interface and electrodes, plays a critical role in determining the performance of all‐polymer solar cells (all‐PSCs), but is often difficult to rationally control. Here, an effective approach for tuning the molecular crystallinity and orientation of naphthalenediimide‐bithiophene‐based n‐type polymers (P(NDI2HD‐T2)) by controlling their number average molecular weights (Mn) is reported. A series of P(NDI2HD‐T2) polymers with different Mn of 13.6 ( PL ), 22.9 ( PM ), and 49.9 kg mol?1 ( PH ) are prepared by changing the amount of end‐capping agent (2‐bromothiophene) during polymerization. Increasing the Mn values of P(NDI2HD‐T2) polymers leads to a remarkable shift of dominant lamellar crystallite textures from edge‐on ( PL ) to face‐on ( PH ) as well as more than a twofold increase in the crystallinity. For example, the portion of face‐on oriented crystallites is dramatically increased from 21.5% and 46.1%, to 78.6% for PL , PM, and PH polymers. These different packing structures in terms of the molecular orientation greatly affect the charge dissociation efficiency at the donor/acceptor interface and thus the short‐circuit current density of the all‐PSCs. All‐PSCs with PTB7‐Th as electron donor and PH as electron acceptor show the highest efficiency of 6.14%, outperforming those with PM (5.08%) and PL (4.29%).  相似文献   

11.
Nonfullerene polymer solar cells (PSCs) are fabricated by using one wide bandgap donor PBDB‐T and one ultranarrow bandgap acceptor IEICO‐4F as the active layers. One medium bandgap donor PTB7‐Th is selected as the third component due to the similar highest occupied molecular orbital level compared to that of PBDB‐T and their complementary absorption spectra. The champion power conversion efficiency (PCE) of PSCs is increased from 10.25% to 11.62% via incorporating 20 wt% PTB7‐Th in donors, with enhanced short‐circuit current (JSC) of 24.14 mA cm?2 and fill factor (FF) of 65.03%. The 11.62% PCE should be the highest value for ternary nonfullerene PSCs. The main contribution of PTB7‐Th can be summarized as the improved photon harvesting and enhanced exciton utilization of PBDB‐T due to the efficient energy transfer from PBDB‐T to PTB7‐Th. Meanwhile, PTB7‐Th can also act as a regulator to adjust PBDB‐T molecular arrangement for optimizing charge transport, resulting in the enhanced FF of ternary PSCs. This experimental result may provide new insight for developing high‐performance ternary nonfullerene PSCs by selecting two well‐compatible donors with different bandgap and one ultranarrow bandgap acceptor.  相似文献   

12.
Significantly increased power conversion efficiency (PCE) of polymer solar cells (PSCs) is achieved by applying a plasmonic enhanced light trapping strategy to a low bandgap conjugated polymer, poly(indacenodithiophene‐ co‐phananthrene‐quinoxaline) (PIDT‐PhanQ) and [6,6]‐phenyl‐C71‐butyric acid methyl ester (PC71BM) based bulk‐heterojunction (BHJ) system. By doping both the rear and front charge‐selecting interfacial layers of the device with different sizes of Au NPs, the PCE of the devices is improved from 6.65% to 7.50% (13% enhancement). A detailed study of processing, characterization, microscopy, and device fabrication is conducted to understand the underlying mechanism for the enhanced device performance. The success of this work provides a simple and generally applicable approach to enhance light harnessing of low bandgap polymers in PSCs.  相似文献   

13.
Poly(benzo[1,2‐b:4,5‐b′]dithiophene–alt–thieno[3,4‐c]pyrrole‐4,6‐dione) (PBDTTPD) polymer donors with linear side‐chains yield bulk‐heterojunction (BHJ) solar cell power conversion efficiencies (PCEs) of about 4% with phenyl‐C71‐butyric acid methyl ester (PC71BM) as the acceptor, while a PBDTTPD polymer with a combination of branched and linear substituents yields a doubling of the PCE to 8%. Using transient optical spectroscopy it is shown that while the exciton dissociation and ultrafast charge generation steps are not strongly affected by the side chain modifications, the polymer with branched side chains exhibits a decreased rate of nongeminate recombination and a lower fraction of sub‐nanosecond geminate recombination. In turn the yield of long‐lived charge carriers increases, resulting in a 33% increase in short circuit current (J sc). In parallel, the two polymers show distinct grazing incidence X‐ray scattering spectra indicative of the presence of stacks with different orientation patterns in optimized thin‐film BHJ devices. Independent of the packing pattern the spectroscopic data also reveals the existence of polymer aggregates in the pristine polymer films as well as in both blends which trap excitons and hinder their dissociation.  相似文献   

14.
The record efficiency of the state‐of‐the‐art polymer solar cells (PSCs) is rapidly increasing, due to the discovery of high‐performance photoactive donor and acceptor materials. However, strong questions remain as to whether such high‐efficiency PSCs can be produced by scalable processes. This paper reports a high power conversion efficiency (PCE) of 13.5% achieved with single‐junction ternary PSCs based on PTB7‐Th, PC71BM, and COi8DFIC fabricated by slot‐die coating, which shows the highest PCE ever reported in PSCs fabricated by a scalable process. To understand the origin of the high performance of the slot‐die coated device, slot‐die coated photoactive films and devices are systematically investigated. These results indicate that the good performance of the slot‐die PSCs can be due to a favorable molecule‐structure and film‐morphology change by introducing 1,8‐diiodooctane and heat treatment, which can lead to improved charge transport with reduced carrier recombination. The optimized condition is then used for the fabrication of large‐area modules and also for roll‐to‐roll fabrication. The slot‐die coated module with 30 cm2 active‐area and roll‐to‐roll produced flexible PSC has shown 8.6% and 9.6%, respectively. These efficiencies are the highest in each category and demonstrate the strong potential of the slot‐die coated ternary system for commercial applications.  相似文献   

15.
The morphology, photophysics, and device performance of solar cells based on the low bandgap polymer poly[[2,6′‐4,8‐di(5‐ethylhexylthienyl)benzo[1,2‐b;3,3‐b]dithiophene]3‐fluoro‐2[(2‐ethylhexyl)carbonyl]thieno[3,4‐b]thiophenediyl (PBDTTT‐EFT) (also known as PTB7‐Th) blended with different fullerene acceptors: Phenyl‐C61‐butyric acid methyl ester (PC61BM), phenyl‐C71 ‐butyric acid methyl ester (PC71BM), or indene‐C60 bisadduct (ICBA) are correlated. Compared to PC71 BM‐based cells – which achieve a power conversion efficiency (PCE) of 9.4% – cells using ICBA achieve a higher open‐circuit voltage (VOC) of 1.0 V albeit with a lower PCE of 7.1%. To understand the origin of this lower PCE, the morphology and photophysics have been thoroughly characterized. Hard and soft X‐ray scattering measurements reveal that the PBDTTT‐EFT:ICBA blend has a lower crystallinity, lower domain purity, and smaller domain size compared to the PBDTTT‐EFT:PC71BM blend. Incomplete photoluminescence quenching is also found in the ICBA blend with transient absorption measurements showing faster recombination dynamics at short timescales. Transient photovoltage measurements highlight further differences in recombination at longer timeframes due to the more intermixed morphology of the ICBA blend. Interestingly, a mild thermal treatment improves the performance of PBDTTT‐EFT:ICBA cells which is exploited in the fabrication of a homo PBDTTT‐EFT:ICBA tandem solar cell with PCE of 9.0% and VOC of 1.93 V.  相似文献   

16.
Efficient conventional bulk heterojunction (BHJ) perovskite hybrid solar cells (pero‐HSCs) solution‐processed from a composite of CH3NH3PbI3 mixed with PC61BM ([6,6]‐phenyl‐C61‐butyric acid methyl ester), where CH3NH3PbI3 acts as the electron donor and PC61BM acts as the electron acceptor, are reported for the first time. The efficiency of 12.78% is twofold enhancement in comparison with the conventional planar heterojunction pero‐HSCs (6.90%) fabricated by pristine CH3NH3PbI3. The BHJ pero‐HSCs are further optimized by using PC61BM/TiO2 bi‐electron‐extraction‐layer (EEL), which are both solution‐processed and then followed with low‐temperature thermal annealing. Due to higher electrical conductivity of PC61BM over that of TiO2, an efficiency of 14.98%, the highest reported efficiency for the pero‐HSCs without incorporating high‐temperature‐processed mesoporous TiO2 and Al2O3 as the EEL and insulating scaffold, is observed from PC61BM modified BHJ pero‐HSCs. Thus, the findings provide a simple way to approach high efficiency low‐cost pero‐HSCs.  相似文献   

17.
The addition of polystyrene (PS), a typical insulator, is empirically shown to increase the power conversion efficiencies (PCEs) of a solution‐deposited bulk heterojunction (BHJ) molecular blend film used in solar cell fabrication: p‐DTS(FBTTh2)2/PC71BM. The performance is further improved by small quantities of diiodooctane (DIO), an established solvent additive. In this study, how the addition of PS and DIO affects the film formation of this bulk heterojunction blend film are probed via in situ monitoring of absorbance, thickness, and crystallinity. PS and DIO additives are shown to promote donor crystallite formation on different time scales and through different mechanisms. PS‐containing films retain chlorobenzene solvent, extending evaporation time and promoting phase separation earlier in the casting process. This extended time is insufficient to attain the morphology for optimal PCE results before the film sets. Here is where the presence of DIO comes into play: its low vapor pressure further extends the time scale of film evolution and allows for crystalline rearrangement of the donor phase long after casting, ultimately leading to the best BHJ organization.  相似文献   

18.
Despite the potential of ternary polymer solar cells (PSCs) to improve photocurrents, ternary architecture is not widely utilized for PSCs because its application has been shown to reduce fill factor (FF). In this paper, a novel technique is reported for achieving highly efficient ternary PSCs without this characteristic sharp decrease in FF by matching the highest occupied molecular orbital (HOMO) energy levels of two donor polymers. Our ternary device—made from a blend of wide‐bandgap poly[4,8‐bis(2‐ethylhexyloxy)benzo[1,2‐b:4,5‐b′]dithiophene‐alt‐2,5‐dioctyl‐4,6‐di(thiophen‐2‐yl)pyrrolo[3,4‐c]pyrrole‐1,3(2H,5H)‐dione) (PBDT‐DPPD) polymer, narrow‐bandgap poly[4,8‐bis[5‐(2‐ethylhexyl)‐2‐thienyl]benzo[1,2‐b:4,5‐b′]dithiophene‐alt‐(4‐(2‐ethylhexyl)‐3‐fluorothieno[3,4‐b]thiophene‐)‐2‐carboxylate‐2‐ 6‐diyl)] (PTB7‐Th) polymer, and [6,6]‐phenyl C70‐butyric acid methyl ester (PC70BM)—exhibits a maximum power conversion efficiency of 10.42% with an open‐circuit voltage of 0.80 V, a short‐circuit current of 17.61 mA cm?2, and an FF of 0.74. In addition, this concept is extended to quaternary PSCs made by using three different donor polymers with similar HOMO levels. Interestingly, the quaternary PSCs also yield a good FF (≈0.70)—similar to those of corresponding binary PSCs. This study confirms that the HOMO levels of the polymers used on the photoactive layer of PSCs are a crucial determinant of a high FF.  相似文献   

19.
The best performing low bandgap copolymers PTB series to date which is based on thieno[3,4‐b]thiophene‐alt‐benzodithiophene units blended with [6,6]‐phenyl‐C71‐butyric acid methyl ester (PC71BM), have been the focus of polymer‐based solar cells. Here, novel fluorinated polymers PTB7‐Fx (fluorine units coupled with submonomer thieno[3,4‐b]thiophene) with varied degree of fluorination are used as electron donor materials. The PTB7‐Fx:PC71BM bulk heterojunction (BHJ) films spin‐coated from the host solvent chlorobenzene without and with solvent additive 1,8‐diiodooctane (DIO) and the corresponding solar cell devices are systematically investigated to address the morphology‐efficiency relationship. Self‐assembled BHJ morphology is already observed for as‐spun blend films. After adding the solvent additive DIO, the pronounced ordered structures are suppressed and better intermixed films with much smaller domain sizes result. Full fluorination of the third C‐atom of thienothiophene gives rise to the highest power conversion efficiency. As the absorption properties, film morphology and crystallinity remain similar for different degrees of fluorination, the main influence of the photovoltaic performance is ascribed to the different lowest unoccupied molecular orbital (LUMO) of each polymer instead of the film morphology. Thus the device performance can be efficiently improved by tuning the energy level of the polymer without necessarily changing either the film nanomorphology or crystallinity dramatically.  相似文献   

20.
Highly efficient tandem and semitransparent (ST) polymer solar cells utilizing the same donor polymer blended with [6,6]‐phenyl‐C61‐butyric acid methyl ester (PC61BM) and [6,6]‐phenyl‐C71‐butyric acid methyl ester (PC71BM) as active layers are demonstrated. A high power conversion efficiency (PCE) of 8.5% and a record high open‐circuit voltage of 1.71 V are achieved for a tandem cell based on a medium bandgap polymer poly(indacenodithiophene‐co‐phananthrene‐quinoxaline) (PIDT‐phanQ). In addition, this approach can also be applied to a low bandgap polymer poly[2,6‐(4,4‐bis(2‐ethylhexyl)‐4H‐cyclopenta[2,1‐b;3,4‐b′]dithiophene)‐alt‐4,7‐(5‐fluoro‐2,1,3‐benzothia‐diazole)] (PCPDTFBT), and PCEs up to 7.9% are achieved. Due to the very thin total active layer thickness, a highly efficient ST tandem cell based on PIDT‐phanQ exhibits a high PCE of 7.4%, which is the highest value reported to date for a ST solar cell. The ST device also possesses a desirable average visible transmittance (≈40%) and an excellent color rendering index (≈100), permitting its use in power‐generating window applications.  相似文献   