Regenerated silk fibroin materials show properties dependent on the methods used to process them. The molecular structures of B. mori silk fibroin both in solution and in solid states were studied and compared using X-ray diffraction, FTIR, and (13)C NMR spectroscopy. Some portion of fibroin protein molecules dissolved in formic acid already have a beta-sheet structure, whereas those dissolved in TFA have some helical conformation. Moreover, fibroin molecules were spontaneously assembled into an ordered structure as the acidic solvents were removed from the fibroin-acidic solvent systems. This may be responsible for the improved physical properties of regenerated fibroin materials from acidic solvents. Regenerated fibroin materials have shown poor mechanical properties and brittleness compared to their original form. These problems were technically solved by improving the fiber forming process according to a method reported here. The regenerated fibroin fibers showed much better mechanical properties compared to the native silk fiber and their physical and chemical properties were characterized by X-ray diffraction, solid state (13)C NMR spectroscopy, SinTech tensile testing, and SEM.  相似文献   

2.
Zhang C  Song D  Lu Q  Hu X  Kaplan DL  Zhu H 《Biomacromolecules》2012,13(7):2148-2153
Although natural silk fibers have excellent strength and flexibility, the regenerated silk materials generally become brittle in the dry state. How to reconstruct the flexibility for silk fibroin has bewildered scientists for many years. In the present study, the flexible regenerated silk fibroin films were achieved by simulating the natural forming and spinning process. Silk fibroin films composed of silk I structure were first prepared by slow drying process. Then, the silk fibroin films were stretched in the wet state, following the structural transition from silk I to silk II. The difference between the flexible film and different brittle regenerated films was investigated to reveal the critical factors in regulating the flexibility of regenerated silk materials. Compared with the methanol-treated silk films, although having similar silk II structure and water content, the flexible silk films contained more bound water rather than free water, implying the great influence of bound water on the flexibility. Then, further studies revealed that the distribution of bound water was also a critical factor in improving silk flexibility in the dry state, which could be regulated by the nanoassembly of silk fibroin. Importantly, the results further elucidate the relation between mechanical properties and silk fibroin structures, pointing to a new mode of generating new types of silk materials with enhanced mechanical properties in the dry state, which would facilitate the fabrication and application of regenerated silk fibroin materials in different fields.  相似文献   

3.
Structure and properties of silk hydrogels   总被引:8,自引:0,他引:8  
Control of silk fibroin concentration in aqueous solutions via osmotic stress was studied to assess relationships to gel formation and structural, morphological, and functional (mechanical) changes associated with this process. Environmental factors potentially important in the in vivo processing of aqueous silk fibroin were also studied to determine their contributions to this process. Gelation of silk fibroin aqueous solutions was affected by temperature, Ca(2+), pH, and poly(ethylene oxide) (PEO). Gelation time decreased with increase in protein concentration, decrease in pH, increase in temperature, addition of Ca(2+), and addition of PEO. No change of gelation time was observed with the addition of K(+). Upon gelation, a random coil structure of the silk fibroin was transformed into a beta-sheet structure. Hydrogels with fibroin concentrations >4 wt % exhibited network and spongelike structures on the basis of scanning electron microscopy. Pore sizes of the freeze-dried hydrogels were smaller as the silk fibroin concentration or gelation temperature was increased. Freeze-dried hydrogels formed in the presence of Ca(2+) exhibited larger pores as the concentration of this ion was increased. Mechanical compressive strength and modulus of the hydrogels increased with increase in protein concentration and gelation temperature. The results of these studies provide insight into the sol-gel transitions that silk fibroin undergoes in glands during aqueous processing while also providing important insight in the in vitro processing of these proteins into useful new materials.  相似文献   

4.
Bombyx mori silk fibers were dissolved in N-methyl morpholine N-oxide (MMNO), an organic cyclic amine oxide used for the solvent spinning of regenerated cellulosic fibers. The commercial MMNO monohydrate used in this study as a solvent for silk is a hygroscopic compound crystalline at room temperature, which becomes an active solvent after melting at 76 degrees C. The degree of hydration of MMNO was checked by DSC measurements. The solvation power of MMNO towards silk fibroin drastically decreased at a water content > or = 20-21% w/w. Dissolution of silk required both thermal and mechanical energy. The optimum temperature was 100 degrees C. At lower temperatures dissolution proceeded very slowly. At higher temperatures, rapid depolymerization of silk fibroin occurred. The value of the Flory-Huggins interaction parameter chi for the MMNO-H2O-silk fibroin system was -8.5, suggesting that dissolution is a thermodynamically favored process. The extent of degradation of silk fibroin was assessed by measuring the intrinsic viscosity and determining the amino acid composition of silk after regeneration with an aqueous methanol solution, which was effective in removing the solvent and coagulating silk. Regenerated silk fibroin membranes were characterized by infrared spectroscopy, differential scanning calorimetry and scanning electron microscopy. The prevailing molecular conformation of silk fibroin chains was the beta-sheet structure, as shown by the intense amide I-III bands at 1704, 1627, 1515, 1260, and 1230 cm(-1). The value of the I1260/I1230 intensity ratio (crystallinity index) was 0.68, comparable to that of the fibers. The DSC thermogram was characteristic of a silk fibroin material with unoriented beta-sheet crystalline structure, with an intense decomposition endotherm at 294 degrees C. The SEM examination of fractured surfaces showed the presence of a dense microstructure with a very fine texture formed by densely packed roundish particles of about 100-200 nm diameter.  相似文献   

5.
In the present work, different biopolymer blend scaffolds based on the silk protein fibroin from Bombyx mori (BM) were prepared via freeze‐drying method. The chemical, structural, and mechanical properties of the three dimensional (3D) porous silk fibroin (SF) composite scaffolds of gelatin, collagen, and chitosan as well as SF from Antheraea pernyi (AP) and the recombinant spider silk protein spidroin (SSP1) have been systematically investigated, followed by cell culture experiments with epithelial prostate cancer cells (LNCaP) up to 14 days. Compared to the pure SF scaffold of BM, the blend scaffolds differ in porous morphology, elasticity, swelling behavior, and biochemical composition. The new composite scaffold with SSP1 showed an increased swelling degree and soft tissue like elastic properties. Whereas, in vitro cultivation of LNCaP cells demonstrated an increased growth behavior and spheroid formation within chitosan blended scaffolds based on its remarkable porosity, which supports nutrient supply matrix. Results of this study suggest that silk fibroin matrices are sufficient and certain SF composite scaffolds even improve 3D cell cultivation for prostate cancer research compared to matrices based on pure biomaterials or synthetic polymers.  相似文献   

6.
Degradation mechanism and control of silk fibroin   总被引:1,自引:0,他引:1  
Lu Q  Zhang B  Li M  Zuo B  Kaplan DL  Huang Y  Zhu H 《Biomacromolecules》2011,12(4):1080-1086
Controlling the degradation process of silk is an important and interesting subject in the field of biomaterials. In the present study, silk fibroin films with different secondary conformations and nanostructures were used to study degradation behavior in buffered protease XIV solution. Different from previous studies, silk fibroin films with highest β-sheet content achieved the highest degradation rate in our research. A new degradation mechanism revealed that degradation behavior of silk fibroin was related to not only crystal content but also hydrophilic interaction and then crystal-noncrystal alternate nanostructures. First, hydrophilic blocks of silk fibroin were degraded. Then, hydrophobic crystal blocks that were formerly surrounded and immobilized by hydrophilic blocks became free particles and moved into solution. Therefore, on the basis of the mechanism, which enables the process to be more controllable and flexible, controlling the degradation behavior of silk fibroin without affecting other performances such as its mechanical or hydrophilic properties becomes feasible, and this would greatly expand the applications of silk as a biomedical material.  相似文献   

7.
In this paper, the spinnable regenerated silk fibroin aqueous solution with high concentration was prepared and the regenerated silk fibers were obtained from the aqueous solution by two different spinning processes at ambient temperature. The orientation of these fibers was characterized by polarizing microscope. Their secondary structure was investigated by Raman spectroscopy and related mechanical properties were also measured. These data showed that shearing is an important step for increasing orientation and silk II (β-sheet) structure, and the mechanical properties of the regenerated silk fibers can also be improved by shearing.  相似文献   

8.
目的:磷酸钙骨水泥(Calcium phosphate cement,CPC)以其诸多优点正得到了越来越多的应用,但其较差的力学性能表现也限制了它的使用范围。本研究目的在于改善磷酸钙骨水泥的力学性能,同时评估改性后的磷酸钙骨水泥的其他性能。方法:通过丝素蛋白(Silk fibroin,SF)的矿化自组装方法制备丝素蛋白/羟基磷灰石复合物(silk fibroin/hydroxyapitite composite, SF/HA)。按照1%、2%、3%、4%的质量分数加入磷酸钙骨水泥中,与磷酸钙骨水泥组对比。比较内容包括力学强度、抗渍散性能及细胞毒性。结果:以丝素蛋白溶液为液相组的磷酸钙骨水泥强度大约为35MPa。随后随着添加丝素蛋白/羟基磷灰石复合物的质量分数从1%增至3%,磷酸钙骨水泥的强度逐渐增加(P〈0.05),最高约至45MPa。而当丝素蛋白/羟基磷灰石的质量分数达到4%时,磷酸钙骨水泥的强度较质量分数3%组小幅度下降至43MPa(P〈0.05)。以丝素蛋白溶液作为液相时,磷酸钙骨水泥的抗溃散能力也得到了加强。在MTT法测定细胞活力的对照实验中,无论是加入丝素蛋白溶液或丝素蛋白/羟基磷灰石复合物,都未观察到细胞毒性。结论:在磷酸钙骨水泥中加入3%质量分数的丝素蛋白/羟基磷灰石复合物,能显著提高磷酸钙骨水泥的抗压强度。而丝素蛋白溶液作为液相可改善磷酸钙骨水泥的抗溃散能力。同时,丝素蛋白和丝素蛋白/羟基磷灰石复合物都不表现出细胞毒性。更理想的力学强度和更强的抗溃散能力,大大扩展了磷酸钙骨水泥的应用范围。  相似文献   

9.
Chen X  Shao Z  Knight DP  Vollrath F 《Proteins》2007,68(1):223-231
Time-resolved FTIR analysis was used to monitor the conformation transition induced by treating regenerated Bombyx mori silk fibroin films and solutions with different concentrations of ethanol. The resulting curves showing the kinetics of the transition for both films and fibroin solutions were influenced by the ethanol concentration. In addition, for silk fibroin solutions the protein concentration also had an effect on the kinetics. At low ethanol concentrations (for example, less than 40% v/v in the case of film), films and fibroin solutions showed a phase in which beta-sheets slowly formed at a rate dependent on the ethanol concentration. Reducing the concentration of the fibroin in solutions also slowed the formation of beta-sheets. These observations suggest that this phase represents a nucleation step. Such a nucleation phase was not seen in the conformation transition at ethanol concentrations > 40% in films or > 50% in silk fibroin solutions. Our results indicate that the ethanol-induced conformation transition of silk fibroin in films and solutions is a three-phase process. The first phase is the initiation of beta-sheet structure (nucleation), the second is a fast phase of beta-sheet growth while the third phase represents a slow perfection of previously formed beta-sheet structure. The nucleation step can be very fast or relatively slow, depending on factors that influence protein chain mobility and intermolecular hydrogen bond formation. The findings give support to the previous evidence that natural silk spinning in silkworms is nucleation-dependent, and that silkworms (like spiders) use concentrated silk protein solutions, and careful control of the pH value and metallic ion content of the processing environment to speed up the nucleation step to produce a rapid conformation transition to convert the water soluble spinning dope to a tough solid silk fiber.  相似文献   

10.
Natural polymers offer various advantages in cartilage tissue engineering applications, thanks to their intrinsic bioactivity and adaptability, which can be exploited for the optimization of scaffold properties. In particular, silk fibroin has multifunctional features driven by the self-assembly of molecular subunits in appropriate environmental conditions. For these reasons, it was used in combination with hyaluronic acid to produce porous sponges for cartilage regeneration. The added amount of hyaluronic acid and the cross-linking with genipin modulated scaffold properties in a synergistic way, showing a strong inter-correlation among macroscopic and microscopic characteristics. Interestingly, hyaluronic acid affected silk fibroin conformation and induced a physical separation between the two material components in absence of genipin. Instead, this was prevented by the cross-linking reaction, resulting in a more interspersed network of protein and polysaccharide molecules partially resembling the structure of cartilage extracellular matrix. In addition, the systematic evaluation of sponge properties and how they can be modulated will represent a significant starting point for the interpretation of the complex outcomes driven by the scaffold in vitro and in vivo.  相似文献   

11.
A system was designed to utilize silk fibroin (SF) as a matrix for wound dressing. For this system, we prepared a sponge type of porous semi-interpenetrating networks (SIPNs) hydrogel composed of SF and poloxamer 407 macromer to enhance the mechanical and functional properties of SF. The thermal and mechanical properties of the hydrogels as well as their swelling behaviors were studied by means of differential scanning calorimetry, compressive modulus measurement, and gravimetric method, respectively. The morphology and crystalline structure of these SIPN hydrogels were also investigated by scanning electron microscopy (SEM) and wide-angle diffractometry, respectively. Conformational change of SF from random coil to beta-sheet structure was accelerated by formation of SIPNs with poloxamer. The melting temperature of poloxamer in the SIPNs decreased due to the prevention of crystallization by the incorporation of SF. The mechanical strength of SIPNs hydrogel was much higher than those of SF itself or SF/poloxamer blend and increased with the poloxamer content. The equilibrium water content of SF was remarkably increased by formation of SIPNs with poloxamer due to the hydrophilicity of poloxamer. The crystallinity and morphology of SIPNs hydrogel were affected by SIPNs hydrogel composition.  相似文献   

12.
Using the tissue-engineered constructs based on scaffolds that imitate the extracellular matrix of living tissues unveils new opportunities in the treatment of various pathologies and injuries associated with tissue and organ damage. Silk fibroin of silkworm Bombyx mori is a biocompatible and bioresorbable polymer with high mechanical strength and elasticity that allows creating scaffolds on its basis for regeneration of various tissues, including bone. In the present work, fibroin scaffolds were obtained. They were designed in the form of porous sponges, films, and hybrid scaffolds of a bilayer structure in which the porous sponge threedimensional structure is limited on one side by a film. The structure of the scaffolds and their biocompatibility were studied: immortalized and primary fibroblasts, as well as the osteoblast-like cells, have been shown to successfully adhere and proliferate on the surface of the studied scaffolds. Numerous osteogenesis foci have been observed in the implant region 4 weeks after the fibroin porous scaffold implantation in the in vivo experiments in a rat femoral bone defect model indicating the osteoconduction of the scaffolds.  相似文献   

13.
Porous 3-D scaffolds from regenerated silk fibroin   总被引:13,自引:0,他引:13  
Three fabrication techniques, freeze-drying, salt leaching and gas foaming, were used to form porous three-dimensional silk biomaterial matrixes. Matrixes were characterized for morphological and functional properties related to processing method and conditions. The porosity of the salt leached scaffolds varied between 84 and 98% with a compressive strength up to 175 +/- 3 KPa, and the gas foamed scaffolds had porosities of 87-97% and compressive strength up to 280 +/- 4 KPa. The freeze-dried scaffolds were prepared at different freezing temperatures (-80 and -20 degrees C) and subsequently treated with different concentrations (15 and 25%) and hydrophilicity alcohols. The porosity of these scaffolds was up to 99%, and the maximum compressive strength was 30 +/- 2 KPa. Changes in silk fibroin structure during processing to form the 3D matrixes were determined by FT-IR and XrD. The salt leached and gas foaming techniques produced scaffolds with a useful combination of high compressive strength, interconnected pores, and pore sizes greater than 100 microns in diameter. The results suggest that silk-based 3D matrixes can be formed for utility in biomaterial applications.  相似文献   

14.
采用酪氨酸酶对丝素蛋白催化氧化,考察了酶促氧化反应对丝素蛋白结构及丝素膜性能的影响。研究结果表明,酪氨酸酶可催化氧化丝素蛋白中酪氨酸残基生成多巴和多巴醌结构衍生物,并且两者含量随催化反应时间延长呈波动性变化;酶促反应后丝素蛋白中游离氨基含量下降,丝素风干膜断裂强度增加,表明酶促氧化中丝素大分子间发生自交联。XRD结果表明酪氨酸酶催化氧化对丝素蛋白二级结构有一定影响;SEM显示酶促改性可能影响丝素蛋白冷冻干燥膜多孔形态结构。  相似文献   

15.
Antheraea pernyi silk fibroin fibers were dissolved by aqueous lithium thiocyanate to obtain regenerated A. pernyi silk fibroin solution. By means of circular dichroism, 13C NMR and Raman spectroscopy, the molecular conformation of regenerated A. pernyi silk fibroin in aqueous solution was investigated. The relationship of environmental factors and sol–gel transformation behavior of regenerated A. pernyi silk fibroin was also studied. The molecular conformations of regenerated A. pernyi silk fibroin mainly were -helix and random coil in solution. There also existed a little β-sheet conformation. It was obviously different with Bombyx mori silk fibroin, whose molecular conformation in solution was only random coil but no -helix existence. With the increase of temperature and solution concentration and with the decrease of solution pH value, the gelation velocity of regenerated A. pernyi silk fibroin solution increased. Especially, it showed that A. pernyi silk fibroin was more sensitive to temperature than B. mori silk fibroin during the sol–gel transformation. The velocity increased obviously when the temperature was above 30 °C. During the sol–gel transformation, the molecular conformation of regenerated A. pernyi silk fibroin changed from random coil to β-sheet structure. The results of these studies provided important insight into the preparation of new biomaterials by silk fibroin protein.  相似文献   

16.
A few bacterial species, mostly gram-negatives, were found to attach themselves and grow on silk buried in soil. On the contrary, no fungi were isolated in such experiments. Growth was more abundant on raw silk (composed of sericin and fibroin) than on degummed silk (fibroin only) indicating that the majority of these bacteria use sericin rather than fibroin for growth. Electron microscopy demonstrated that bacteria formed a biofilm on the fabric and caused extensive damage to the fibers resulting in considerable reduction in the mechanical properties. Of the three main bacterial species isolated from silk exposed to soil or by enrichment cultures of silk cocoons, only Pseudomonas (Burkholderia) cepacia appeared to be able to use fibroin as a sole source of carbon and nitrogen for growth. Indeed, in laboratory experiments, pure cultures of P. cepacia were found to form a well-developed biofilm on fibroin, to hydrolyze fibroin, and to produce an extracellular enzyme attacking this protein. The reported data indicate that bacteria but not fungi may attack and degrade silk proteins and thus cause irreversible damage to silk artifacts of artistic or historical interest.  相似文献   

17.
为了进一步提高伤口敷料的止血性能,文中在生物相容性良好的壳聚糖溶液中引入含有多种生长因子的人源性富血小板血浆(Humanplatelet-richplasma,hPRP),并加入不同体积比例(1∶1、1∶3、3∶1、1∶0)的丝素蛋白溶液以提高材料的多孔性与止血性,通过冷冻干燥法制备不同配比的hPRP-壳聚糖/丝素蛋白敷料,并将纯壳聚糖敷料作为对照组,研究hPRP和丝素蛋白对敷料的止血性能的影响以及丝素蛋白对PRP中生长因子控制释放的影响。结果表明,在壳聚糖敷料中引入hPRP对敷料的止血性有所提高,但对敷料的多孔结构及吸水率无明显改善,若在hPRP-壳聚糖溶液中按照体积比为1∶1的比例加入丝素蛋白溶液,会得到具有较为均匀的多孔结构的敷料,敷料的孔隙率与吸水率分别可达到86.83%±3.84%与1 474%±114%,且该比例的敷料在快速止血性能上表现优异。此外,加入丝素蛋白与壳聚糖比例为1∶1的PRP敷料能有效减少PRP中生长因子在初始阶段的爆裂释放。因此,含hPRP的壳聚糖/丝素蛋白复合敷料有望成为一种能快速止血且能促进伤口愈合的新型伤口敷料。  相似文献   

18.

Background

Bombyx mori silk fibers with thin diameters have advantages of lightness and crease-resistance. Many studies have used anti-juvenile hormones to induce trimolters in order to generate thin silk; however, there has been comparatively little analysis of the morphology, structure and mechanical properties of trimolter silk.

Methods

This study induced two kinds of trimolters by appling topically anti-juvenile hormones and obtained thin diameter silk. Scanning electron microscope (SEM), FTIR analysis, tensile mechanical testing, chitin staining were used to reveal that the morphology, conformation and mechanical property of the trimolter silk.

Results

Cocoon of trimolters were highly densely packed by thinner fibers and thus had small apertures. We found that the conformation of trimolter silk fibroin changed and formed more β-sheet structures. In addition, analysis of mechanical parameters yielded a higher Young's modulus and strength in trimolter silk than in the control. By chitin staining of silk gland, we postulated that the mechanical properties of trimolters' silk was enhanced greatly during to the structural changes of silk gland.

Conclusion

We induced trimolters by anti-juvenile hormones and the resulting cocoons were more closely packed and had smaller silk fiber diameters. We found that the conformation of trimolters silk fibroin had a higher content of β-sheet structures and better mechanical properties.

General significance

Our study revealed the structures and mechanical properties of trimolter silk, and provided a valuable reference to improve silk quality by influencing molting in silkworms.  相似文献   

19.
Silk has a long history of use in medicine as sutures. To address the requirements of a mechanically robust and biocompatible material, basic research to clarify the role of repeated sequences in silk fibroin in its structures and properties seems important as well as the development of a processing technique suitable for the preparation of fibers with excellent mechanical properties. In this study, three silk-like protein analogs were constructed from two regions selected from among the crystalline region of Bombyx mori silk fibroin, (GAGSGA)(2), the crystalline region of Samia cynthia ricini silk fibroin, (Ala)(12), the crystalline region of spider dragline silk fibroin, (Ala)(6), and the Gly-rich region of spider silk fibroin, (GGA)(4). The silk-like protein analog constructed from the crystalline regions of the spider dragline silk and B. mori silk fibroins, (A(6)SCS)(8), that constructed from the crystalline regions of the S. c.ricini and B. mori silk fibroins, (A(12)SGS)(4), that constructed from and the crystalline region of S. c.ricini silk fibroin and the glycine-rich region of spider dragline silk fibroin, (A(12)SGS)(4),were expressed their molecular weights being about 36.0 kDa, 17.0 kDa and 17.5 kDa, respectively in E. coli by means of genetic engineering technologies. (A(12)SCS)(4) and (A(12)SGS)(4 )undergo a structural transition from alpha-helix to beta-sheet on a change in the solvent treatment from trifluoroacetic acid (TFA) to formic acid (FA). However, (A(6)SCS)(8) takes on the beta-sheet structure predominantly on TFA treatment and FA treatment. Structural analysis was performed on model peptides selected from spider dragline and S. c.ricini silks by means of (13)C CP/MAS NMR.  相似文献   

20.
Horseradish peroxide (HRP) was covalently coupled to three-dimensional (3D) silk fibroin scaffolds using water-soluble carbodiimide. Stable, bilaterally symmetrical immobilized HRP gradient patterns were generated within 3D silk fibroin scaffolds using the principles of diffusion. Gradients of immobilized HRP activity were controlled using variables of volume and concentration of HRP solution activated by the carbodiimide. The method developed can be extended to immobilize a variety of proteins and small molecules on several types of porous, interconnected materials. This technique of patterning enzymes and proteins in a gradient manner offers new options in the field of chemotaxis, tissue engineering, and biosensors.  相似文献   