1.
Fouling-release coatings were prepared from blends of a fluorinated/siloxane copolymer with a poly(dimethyl siloxane) (PDMS) matrix in order to couple the low modulus character of PDMS with the low surface tension typical for fluorinated polymers. The content of the surface-active copolymer was varied in the blend over a broad range (0.15–10 wt % with respect to PDMS). X-ray photoelectron spectroscopy depth profiling analyses were performed on the coatings to establish the distribution of specific chemical constituents throughout the coatings, and proved enrichment in fluorine of the outermost layers of the coating surface. Addition of the fluorinated/siloxane copolymer to the PDMS matrix resulted in a concentration-dependent decrease in settlement of barnacle, Balanus amphitrite, cyprids. The release of young plants of Ulva, a soft fouling species, and young barnacles showed that adhesion strength on the fluorinated/siloxane copolymer was significantly lower than the siloxane control. However, differences in adhesion strength were not directly correlated with the concentration of copolymer in the blends.  相似文献   

2.

This study compared the shear adhesion strength of barnacles, oysters and tubeworms on eight RTV 11‐based silicone fouling‐release coatings containing different silicone oil additives. It was found that adhesion strength differed among species and coating types. In most cases, oysters and tubeworms had higher adhesion strengths than barnacles. Barnacle adhesion strength was reduced on all coatings containing oil additives; however, this was not generally true for oysters and tubeworms. The difference in the adhesion strength among the three organisms tested in this study emphasizes the importance of understanding the fundamental interaction between marine invertebrate adhesives and the substratum.  相似文献   

3.

Fouling-release coatings prevent fouling of ships' hulls through hydrodynamic forces generated as the ship moves through the water. The effectiveness of such coatings may be evaluated by measuring the adhesion strength of settled organisms, e.g. barnacles. The influence of desiccation of the barnacle adhesive on such measurements was investigated. Shear forces required to remove barnacles of the genus Balanus increased during the course of desiccation up to the point when the barnacles suddenly self-detached. The increase was thought to be due to the rising cohesive strength of the adhesive. Growing tensile forces within the weakly cross-linked adhesive, however, are suggested to have led to self-detachment. The shear forces required to remove barnacles of the genus Elminius were generally low and did not differ significantly during the course of desiccation. The different results may be attributed to specific base morphologies. It was concluded that measuring the adhesion strength of members of the Balanidae on non-stick surfaces in air could produce flawed results due to the influence of desiccation of the barnacle adhesive. The investigations have also provided new insights into the characteristics of barnacle adhesive.  相似文献   

4.
Abstract

A high-throughput bacterial biofilm retention screening method has been augmented to facilitate the rapid analysis and down-selection of fouling-release coatings for identification of promising candidates. Coatings were cast in modified 24-well tissue culture plates and inoculated with the marine bacterium Cytophaga lytica for attachment and biofilm growth. Biofilms retained after rinsing with deionised water were dried at ambient laboratory conditions. During the drying process, retained biofilms retracted through a surface de-wetting phenomenon on the hydrophobic silicone surfaces. The retracted biofilms were stained with crystal violet, imaged, and analysed for percentage coverage. Two sets of experimental fouling-release coatings were analysed with the high-throughput biofilm retention and retraction assay (HTBRRA). The first set consisted of a series of model polysiloxane coatings that were systematically varied with respect to ratios of low and high MW silanol-terminated PDMS, level of cross-linker, and amount of silicone oil. The second set consisted of cross-linked PDMS-polyurethane coatings varied with respect to the MW of the PDMS and end group functionality. For the model polysiloxane coatings, HTBRRA results were compared to data obtained from field immersion testing at the Indian River Lagoon at the Florida Institute of Technology. The percentage coverage calculations of retracted biofilms correlated well to barnacle adhesion strength in the field (R2 = 0.82) and accurately identified the best and poorest performing coating compositions. For the cross-linked PDMS-polyurethane coatings, the HTBRRA results were compared to combinatorial pseudobarnacle pull-off adhesion data and good agreement in performance was observed. Details of the developed assay and its implications in the rapid discovery of new fouling-release coatings are discussed.  相似文献   

5.
Abstract

Poly(dimethylsiloxane) (PDMS) elastomer coatings containing an amphiphilic hydrolyzable diblock copolymer additive were prepared and their potential as marine antifouling and antiadhesion materials was tested. The block copolymer additive consisted of a PDMS first block and a random poly(trialkylsilyl methacrylate (TRSiMA, R?=?butyl, isopropyl)-co-poly(ethyleneglycol) methacrylate (PEGMA) copolymer second block. PDMS-b-TRSiMA block copolymer additives without PEGMA units were also used as additives. The amphiphilic character of the coating surface was assessed in water using the captive air bubble technique for measurements of static and dynamic contact angles. The attachment of macro- and microorganisms on the coatings was evaluated by field tests and by performing adhesion tests to the barnacle Amphibalanus amphitrite and the green alga Ulva rigida. All the additive-based PDMS coatings showed better antiadhesion properties to A. amphitrite larvae than to U. rigida spores. Field tests provided meaningful information on the antifouling and fouling release activity of coatings over an immersion period of 23?months.  相似文献   

6.

Little is known about the performance of fouling‐release coatings at different geographical locations. An investigation was designed to measure the differences in biofouling and biofouling adhesion strength on three known silicone formulations and an epoxy control at seven static immersion sites located in California, Florida, Hawaii, Hong Kong, India, Italy and Singapore. The study found that whilst the relative performance of the coatings was similar at each site, there were statistically significant differences in the type and intensity of fouling that developed on the coatings and in barnacle adhesion strength among sites. The results emphasize the importance of evaluating potential coatings at more than one static immersion site.  相似文献   

7.
A number of factors affect the adhesion strength of organisms to fouling-release coatings, and except for a few studies focussing on black or white surfaces none have dealt specifically with the effect of coating colour. The aim was to test the effect of colour on the adhesion strength of the barnacle Elminius modestus. Panels coated in six commercial colours of Intersleek 700® were submerged at two field sites and barnacles were pushed-off using a standard assay procedure. The strength of adhesion (SOA) varied between and within sites for colour and by barnacle basal area, SOA per unit area being higher for smaller barnacles. Higher SOA with a small basal area may be because of size-specific predation, differential hydrodynamic effects or adhesive failure with age. The complex effect of colour on barnacle adhesion may be because of physico-chemical surface characteristics varying with pigments, and their interactions with local environmental conditions, as well as interactions with the settling barnacle larvae.  相似文献   

8.
Fouling species produce adhesive polymers during the settlement, adhesion and colonization of new surfaces in the marine environment. The present paper tests the hypothesis that enzymes of the appropriate specificity may prevent biofouling by hydrolysing these adhesive polymers. Seventeen commercially available enzyme preparations designed originally for bulk use in a range of end-use applications were tested for their effects on the settlement and/or adhesion of three major fouling species, viz. the green alga Ulva linza, the diatom Navicula perminuta and the barnacle Balanus amphitrite. The serine-proteases were found to have the broadest antifouling potential reducing the adhesion strength of spores and sporelings of U. linza, cells of N. perminuta and inhibiting settlement of cypris larvae of B. amphitrite. Mode-of-action studies on the serine-protease, Alcalase, indicated that this enzyme reduced adhesion of U. linza in a concentration-dependent manner, that spores of the species could recover their adhesive strength if the enzyme was removed and that the adhesive of U. linza and juvenile cement of B. amphitrite became progressively less sensitive to hydrolysis as they cured.  相似文献   

9.
Barnacle adhesion strength was used to screen seventy-seven polydimethylsiloxane elastomeric coatings for fouling-release properties. The test coatings were designed to investigate the effect on barnacle adhesion strength of silicone fluid additive type, additive location, additive molecular weight, additive loading level, mixtures of additives, coating matrix type and coating fillers. The type of silicone fluid additive was the primary controlling factor in barnacle fouling-release. The type of silicone matrix in which the fluid resided was found to alter the effect on fouling-release. Two PDMS fluids, DMSC15 and DBE224, significantly reduced the adhesion strength of barnacles compared to unmodified elastomers. Optimum fouling-release performance was dependent on the interaction of fluid type and elastomeric matrix.  相似文献   

10.
Fouling-release (FR) coatings minimise the adhesion strength of fouling organisms. This study describes improved technologies to control the settlement and adhesion of the important fouling organism Mytilus galloprovincialis by incorporating the nanofillers titanium dioxide (TiO2) and carbon nanotubes (CNTs) in polydimethylsiloxane (PDMS) matrices. The incorporation of TiO2 prevented larval settlement when photoactivated with UV light, even at the lowest concentration of the nanofiller (3.75 wt%). Notably, there was 100% mortality of pediveligers exposed to photoactivated TiO2. However, plantigrades initially settled to photoactivated TiO2, but their adhesion strength was significantly reduced on these surfaces in comparison to blank PDMS. In addition, plantigrades had high mortality after 6 h. In contrast to the enhanced antifouling and FR properties of PDMS incorporating TiO2, the incorporation of CNTs had no effect on the settlement and adhesion of M. galloprovincialis.  相似文献   

11.
Barnacle adhesion strength was used to screen seventy-seven polydimethylsiloxane elastomeric coatings for fouling-release properties. The test coatings were designed to investigate the effect on barnacle adhesion strength of silicone fluid additive type, additive location, additive molecular weight, additive loading level, mixtures of additives, coating matrix type and coating fillers. The type of silicone fluid additive was the primary controlling factor in barnacle fouling-release. The type of silicone matrix in which the fluid resided was found to alter the effect on fouling-release. Two PDMS fluids, DMSC15 and DBE224, significantly reduced the adhesion strength of barnacles compared to unmodified elastomers. Optimum fouling-release performance was dependent on the interaction of fluid type and elastomeric matrix.  相似文献   

12.
Siloxane–polyurethane fouling-release (FR) coatings based on aminopropyl terminated poly(dimethylsiloxane) (PDMS) macromers were prepared and characterized for FR performance via laboratory biological assays. These systems rely on self-stratification, resulting in a coating with a siloxane-rich surface and polyurethane bulk. Previously, these coating systems have used PDMS with multiple functional groups which react into the polyurethane bulk. Here, aminopropyl terminated PDMS macromers were prepared, where a single amine group anchors the PDMS in the coating. Coatings were prepared with four molecular weights (1000, 5000, 10,000, and 15,000 g mol?1) and two levels of PDMS (5% and 10%). High water contact angles and low surface energies were observed for the coatings before and after water immersion, along with low pseudobarnacle removal forces. Laboratory bioassays showed reduced biofilm retention of marine bacteria, good removal of diatoms from coatings with low molecular weight PDMS, high removal of algal sporelings (young plants), and low removal forces of live barnacles.  相似文献   

13.
The facile preparation of amphiphilic network coatings having a hydrophobic dimethacryloxy-functionalized perfluoropolyether (PFPE-DMA; M w = 1500 g mol?1) crosslinked with hydrophilic monomethacryloxy functionalized poly(ethylene glycol) macromonomers (PEG-MA; M w = 300, 475, 1100 g mol?1), intended as non-toxic high-performance marine coatings exhibiting antifouling characteristics is demonstrated. The PFPE-DMA was found to be miscible with the PEG-MA. Photo-cured blends of these materials containing 10 wt% of PEG-MA oligomers did not swell significantly in water. PFPE-DMA crosslinked with the highest molecular weight PEG oligomer (ie PEG1100) deterred settlement (attachment) of algal cells and cypris larvae of barnacles compared to a PFPE control coating. Dynamic mechanical analysis of these networks revealed a flexible material. Preferential segregation of the PEG segments at the polymer/air interface resulted in enhanced antifouling performance. The cured amphiphilic PFPE/PEG films showed decreased advancing and receding contact angles with increasing PEG chain length. In particular, the PFPE/PEG1100 network had a much lower advancing contact angle than static contact angle, suggesting that the PEG1100 segments diffuse to the polymer/water interface quickly. The preferential interfacial aggregation of the larger PEG segments enables the coating surface to have a substantially enhanced resistance to settlement of spores of the green seaweed Ulva, cells of the diatom Navicula and cypris larvae of the barnacle Balanus amphitrite as well as low adhesion of sporelings (young plants) of Ulva, adhesion being lower than to a polydimethyl elastomer, Silastic T2.  相似文献   

14.
Laboratory experiments were conducted to study the impact of laser irradiation on the larvae of the fouling barnacle Balanus amphitrite. Research pertaining to fouling invertebrate larvae‐laser interaction is sparse and, hence, data on this aspect were thought significant in order to consider pulsed low power laser irradiations as a possible future antifouling tool. Lethal and sub‐lethal impacts of four very low laser fluences, viz. 0.013, 0.025, 0.05 and 0.1 J cm‐2 for three different durations, viz. 2, 10 and 30 s were investigated. Three growth stages of barnacle larvae, viz. nauplii stage II, nauplii stage IV and cyprids were exposed to the mentioned laser fluences for different durations. While lethal impact was assessed immediately after and 1 d after irradiation, sub‐lethal impacts were studied by monitoring the success rate of the irradiated nauplii in reaching the cyprid stage. In addition, the swimming speed of VIth stage nauplii after irradiation was studied. In the case of cyprids, in addition to the mortality measurement immediately after and 1 d after irradiation, the settlement rate was investigated. In all the above experiments, non‐irradiated larvae served as controls. The results showed an increase in mortality with increasing laser fluence and duration of irradiation. Irradiation for 2 s resulted in significant mortality in nauplii, while it was less in the case of cyprids. In IInd stage nauplii, the mortality immediately after irradiation for 2 s varied from 14.8±2.12 to 97.1±4.1% for laser fluences of 0.013 and 0.1 J cm‐2, respectively. However, in cyprids, the mortality immediately after irradiation for 2 s varied from 12.2±3 to 13.4±1.2% for fluences of 0.013 and 0.1 J cm‐2, respectively. The mortality in IVth stage nauplii was less than that for IInd stage nauplii but more than that for cyprids. There was a significant increase in mortality with time after irradiation. The formation of cyprids from the irradiated larvae was significantly less than that observed for non‐irradiated larvae. Also, the irradiated larvae showed a significantly slower swimming speed compared to the control samples. The settlement rate in cyprids was reduced significantly by the laser irradiation. This was true even for the lowest fluence and shortest period of irradiation tested. Thus, the results of the experiment showed that even a low power pulsed laser irradiation of 0.013 J cm‐2 for 2 s can cause significant damage to fouling barnacle larvae.  相似文献   

15.
A laminar flow biofilm-monitoring system was used to determine the efficacies of three antifouling (AF) coatings and five fouling-release (FR) coatings againstVibrio harveyi attachment. On-line measurements of tryptophan fluorescence and bioluminescence from each coating, normalized to an upstream stainless steel coupon, were used to determine the effects of AF and FR surfaces on biofilm formation. The AF coatings consisted of 5, 10, and 35 wt% Sea Nine 211 (C9211) incorporated into a vinyl copolymer. Both the 10 and 35 wt% coatings significantly inhibited biofilm biomass development measured by tryptophan fluorescence compared to the stainless steel control.V. harveyi bioluminescence was significantly greater than tryptophan fluorescence in cells attached to these coatings, suggesting that bioluminescence expression may be a marker for cellular stress or toxicity in biofilms. Five different polydimethylsiloxane (PDMS) FR coatings did not inhibit biofilm formation under low flow conditions. However, four PDMS coatings demonstrated decreased biomass levels compared to stainless steel after exposure to a shear stress of 330 dynes cm–2. There was no toxic additive in these coatings; bioluminescence and tryptophan fluorescence were proportional.  相似文献   

16.
A series of eight novel siloxane-polyurethane fouling-release (FR) coatings were assessed for their FR performance in both the laboratory and in the field. Laboratory analysis included adhesion assessments of bacteria, microalgae, macroalgal spores, adult barnacles and pseudobarnacles using high-throughput screening techniques, while field evaluations were conducted in accordance with standardized testing methods at three different ocean testing sites over the course of six-months exposure. The data collected were subjected to statistical analysis in order to identify potential correlations. In general, there was good agreement between the laboratory screening assays and the field assessments, with both regimes clearly distinguishing the siloxane-polyurethane compositions comprising monofunctional poly(dimethyl siloxane) (PDMS) (m-PDMS) as possessing superior, broad-spectrum FR properties compared to those prepared with difunctional PDMS (d-PDMS). Of the seven laboratory screening techniques, the Cellulophaga lytica biofilm retraction and reattached barnacle (Amphibalanus amphitrite) adhesion assays were shown to be the most predictive of broad-spectrum field performance.  相似文献   

17.

The volatile substance extracted from conspecific adults induces larval settlement of the barnacle Balanus amphitrite. The settlement inducing activity of the volatile fractions was checked monthly from June, 1997 to December, 1998. Both water soluble extracts and volatile fractions from the barnacle were prepared by the steam distillation. The active cue in the volatile fraction was always extracted with n‐pentane under acidic conditions, although settlement inducing activity varied with the sample. GC‐MS analysis of the active and inactive pentane fractions revealed 1, 2, 3‐trimethyl‐benzene as the settlement inducing substance. Commercially available 1, 2, 3‐trimethylbenzene also showed high settlement inducing activity at a concentration of 0.8 × 10‐12 M (100 pg 1‐1). This substance was detected at concentrations of more than 7 ng g‐1 of wet barnacle (equivalent to 0.6 × 10‐12M, equal to 70pg1‐1) by GC analysis. These results indicate that 1,2,3‐trimethylbenzene in the volatile fractions acts as a chemical cue for larval settlement. Monthly variation in the settlement inducing activity was observed, which synchronized with the breeding season of the barnacle. This observation suggests that the barnacle produced the chemical cue in the gonad during maturation or accumulated it from the environment.  相似文献   

18.
Abstract

The adhesion of six fouling organisms: the barnacle Balanus eburneus, the gastropod mollusc Crepidula fornicata, the bivalve molluscs Crassostrea virginica and Ostrea/Dendrostrea spp., and the serpulid tubeworms Hydroides dianthus and H. elegans, to 12 silicone fouling-release surfaces was examined. Removal stress (adhesion strength) varied among the fouling species and among the surfaces. Principal component analysis of the removal stress data revealed that the fouling species fell into two distinct groups, one comprising the bivalve molluscs and tubeworms, and the other the barnacle and the gastropod mollusc. None of the silicone materials generated a minimum in removal stress for all the organisms tested, although several surfaces produced low adhesion strengths for both groups of species. These results suggest that fouling-release materials do not rank (in terms of adhesion strength) identically for all fouling organisms, and thus development of a globally-effective hull coating will continue to require testing against a diversity of encrusting species.  相似文献   

19.
A computer-controlled force gauge designed to measure the adhesive strength of barnacles on test substrata is described. The instrument was evaluated with adult barnacles grown in situ on Silastic T2®-coated microscope slides and epoxy replicas adhered to the same substratum with synthetic adhesive. The force per unit area required to detach the barnacles (critical removal stress) using the new automated system was comparable to that obtained with ASTM D5618 (1994 ASTM D5618. 1994. Standard test method for measurement of barnacle adhesion strength in shear American Standard for Testing and Materials. Paint-Tests for formulated products and applied coatings 06.01 [Google Scholar]) (0.19 and 0.28 MPa compared with 0.18 and 0.27 MPa for two batches of barnacles). The automated method showed a faster rate of force development compared with the manual spring force gauge used for ASTM D5618 (1994 ASTM D5618. 1994. Standard test method for measurement of barnacle adhesion strength in shear American Standard for Testing and Materials. Paint-Tests for formulated products and applied coatings 06.01 [Google Scholar]). The new instrument was as accurate and precise at determining surface area as manual delineation used with ASTM D5618 (1994 ASTM D5618. 1994. Standard test method for measurement of barnacle adhesion strength in shear American Standard for Testing and Materials. Paint-Tests for formulated products and applied coatings 06.01 [Google Scholar]). The method provided significant advantages such as higher throughput speed, the ability to test smaller barnacles (which took less time to grow) and to control the force application angle and speed. The variability in measurements was lower than previously reported, suggesting an improved ability to compare the results obtained by different researchers.  相似文献   

20.
Summary In the present investigation the influence of various soil physical parameters on seeding emergence of corn (Zea mays L.) and their critical limits was studied in order to obtain a proper crop stand. The effect of soil compaction, resulting into various bulk densities on some soil physical properties was also studied. Seedling emergence decreased with increasing bulk density, soil suction, seed placement depth, soil strength and with decreasing oxygen diffusion rates. The critical values for these soil physical parameters were found to be 1.4 g/cm3, 3 atm., 4 cm, 1.0 kg/cm2 and 40×10-8 g O2/cm2/min bulk density, soil suction, seed placement depth, soil strength and oxygen diffusion rates respectively. Increasing bulk density decreased the soil water content, oxygen diffusion rates and increased the soil strength. re]19751117 Soil Science Department  相似文献   